About Carbon Steel, Alloy Steel, Spring Steel, and Cast Iron
More
Hard Wear-Resistant 52100 Alloy Steel Tubes
- Yield Strength: See table
- Hardness: See table
- Heat Treatable: Yes
- Maximum Hardness After Heat Treatment: Rockwell C60
- Specifications Met: ASTM A295
Easier to machine than 52100 alloy steel rods, these extremely hard and wear-resistant tubes are often used to create bearings, bushings, and other cylindrical parts that are under constant stress. They’re also known as chrome steel.
For technical drawings and 3-D models, click on a part number.
Certificates with a traceable lot number are available for these products. Download certificates from ORDER HISTORY after your order ships.
OD | OD Tolerance | ID | ID Tolerance | Yield Strength, psi | Hardness | 1 ft. Lg. | 3 ft. Lg. | 6 ft. Lg. | |
0.245" Wall Thickness (-0.0123" to 0.0123" Tolerance) | |||||||||
---|---|---|---|---|---|---|---|---|---|
1.207" | -0.005" to 0.005" | 0.717" | -0.01" to 0.01" | 140,000 | Rockwell B100 | 0000000 | |||
0.309" Wall Thickness (-0.0155" to 0.0155" Tolerance) | |||||||||
1.315" | -0.005" to 0.005" | 0.697" | -0.01" to 0.01" | 140,000 | Rockwell B100 | 0000000 | |||
0.353" Wall Thickness (-0.0176" to 0.0176" Tolerance) | |||||||||
1.551" | -0.005" to 0.005" | 0.846" | -0.01" to 0.01" | 140,000 | Rockwell B100 | 0000000 | |||
0.382" Wall Thickness (-0.0191" to 0.0191" Tolerance) | |||||||||
2.071" | -0.006" to 0.006" | 1.253" | -0.01" to 0.01" | 140,000 | Rockwell B100 | 0000000 | |||
0.472" Wall Thickness (-0.0236" to 0.0236" Tolerance) | |||||||||
2.57" | -0.008" to 0.008" | 1.627" | -0.01" to 0.01" | 140,000 | Rockwell B100 | 0000000 | |||
0.807" Wall Thickness (-0.061" to 0.061" Tolerance) | |||||||||
3.138" | -0.019" to 0.019" | 1.524" | Not Rated | 50,000 | Rockwell B95 | 0000000 |