Filter by
Hardness
Hardness Rating
Specifications Met
Tolerance Rating
Elongation
Appearance
Heat Treatment
Fabrication
Maximum Hardness After Heat Treatment
Maximum Temperature
REACH
RoHS
System of Measurement
Export Control Classification Number (ECCN)
Magnetic Properties
DFARS Specialty Metals
Heat Treatable
Minimum Temperature
Yield Strength
About Stainless Steel
Compare over 25 types of stainless steel to find the right material for you—all with material certificates for traceability.
Easy-to-Harden 13-8 PH Stainless Steel

- Yield Strength: Not Rated
- Hardness: Rockwell C35 (Hard)
- Heat Treatment: Annealed (Softened)
- Heat Treatable: Yes
- Max. Hardness After Heat Treatment: Not Rated
- Specifications Met: SAE AMS5629
13-8 PH stainless steel can be hardened at lower temperatures than other heat-treatable types of stainless steel. It is widely used for fittings, pins, and lock washers. This material maintains its corrosion resistance in temperatures up to 1100° F.
Dia. | Dia. Tolerance | Fabrication | Straightness Tolerance | Magnetic Properties | 1/2 ft. Lg. | 1 ft. Lg. | 3 ft. Lg. | |
1/4" | -0.001" to 0.001" | Hot Rolled | 0.0125" per ft. | Magnetic | 0000000 | |||
5/16" | -0.002" to 0.002" | Hot Rolled | 0.0125" per ft. | Magnetic | 0000000 | |||
3/8" | -0.002" to 0.002" | Hot Rolled | 0.0125" per ft. | Magnetic | 0000000 | |||
1/2" | -0.002" to 0.002" | Hot Rolled | 0.0125" per ft. | Magnetic | 0000000 | |||
3/4" | -0.002" to 0.002" | Hot Rolled | 0.0125" per ft. | Magnetic | 0000000 | |||
1" | -0.003" to 0.003" | Hot Rolled | 0.0125" per ft. | Magnetic | 0000000 |