High-Temperature Casting Compounds
Capture intricate details when creating prototypes, molds, and linings with these easy-to-mix compounds.
High-purity alumina resists shrinking in casts, has a low level of contamination, and is a strong electrical insulator. It’s often used for constructing furnaces and handling liquid metal.
View our selection of release agents.
Time to Harden | Time to Cure | Time to Demold | Cure Temperature, °F | Max. Temperature, °F | Shrinkage | Color | Mixing Required | Volume, cu. in. | Weight, lbs. | Each | |
High-Purity Alumina | |||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|
25 min. | 24 hrs. | 24 hrs. | 77° | 3200° | 1.3% | White | Yes | 98 | 10 | 0000000 | 0000000 |