McMaster-Carr logo
    Filter by
    Maximum Temperature
    Color
    Environment
    Time to Cure
    Mixing Required
    Time to Harden
    U.S.–Mexico–Canada Agreement (USMCA) Qualifying
    Cure Temperature
    Time to Demold
    DFARS Specialty Metals
    Export Control Classification Number (ECCN)
    Industrial Info Snippet
    Shrinkage
    Enter e-mail addresses in the fields below
    Message
    Cancel
    Comments
    E-mail address (if you would like a response)
    2 Products

    High-Temperature Casting Compounds

    Image of ProductInUse. Front orientation. Casting Compounds.
    Capture intricate details when creating prototypes, molds, and linings with these easy-to-mix compounds.
    View our selection of release agents.
    Silica—Silica withstands rapid changes in temperature without cracking and has a low rate of thermal expansion.
    Time to Harden,
    min.
    Time to
    Cure, hr.
    Time to
    Demold, hr.
    Cure Temp.,
    ° F
    Max. Temp.,
    ° F
    Shrinkage
    Color
    Mixing
    Req.
    Volume,
    cu. in.
    Wt.,
    lb.
    Each
    Silica
    202424772,7001.3%WhiteYes6248498K41000000
    202424772,7001.3%WhiteYes155108498K11000000
     