About Carbon Steel, Alloy Steel, Spring Steel, and Cast Iron
More
View a wire gauge conversion chart.
Low-Carbon Steel Wire
- Heat Treatment: Annealed (Softened)
- Heat Treatable: Yes
- Max. Hardness After Heat Treatment: Not Rated
- Tensile Strength: 70,000 psi
- Specifications Met: ASTM A853
Also known as black-annealed wire, this low-carbon steel wire will stay in place when bent. It's commonly used for bundling and as tag wire. This material can be surface hardened with heat treating.
Container | ||||||||
---|---|---|---|---|---|---|---|---|
Dia. | Dia. Tolerance | Lg., ft. | Color | Max. Temperature, °F | Net Weight, lbs. | Type | Each | |
Matte | ||||||||
0.135" | -0.003" to 0.003" | 20 | Dark Gray | 300° | 1 | Coil | 0000000 | 000000 |
0.135" | -0.003" to 0.003" | 100 | Dark Gray | 300° | 5 | Coil | 0000000 | 00000 |
0.135" | -0.003" to 0.003" | 205 | Dark Gray | 300° | 10 | Coil | 0000000 | 00000 |
0.135" | -0.003" to 0.003" | 2,055 | Dark Gray | 300° | 100 | Coil | 0000000 | 000000 |
1 ft. Lg. | ||||||
---|---|---|---|---|---|---|
Dia. | Dia. Tolerance | Color | Max. Temperature, °F | Pkg. Qty. | Pkg. | |
Matte | ||||||
0.135" | -0.003" to 0.003" | Dark Gray | 300° | 10 | 0000000 | 000000 |
Zinc-Galvanized Steel Wire
- Heat Treatment: Annealed (Softened)
- Heat Treatable: No
- Tensile Strength: 70,000 psi
- Specifications Met: ASTM A641
This wire is zinc galvanized for good corrosion resistance. It will stay in place when bent and is commonly used for bundling and as tag wire.